CLAY BODY BLACK 376 10 kg
Throwing and hand-building body
Price with VAT:
18,30 €
Firing colour
brown-black
Chamotte (grain size)
0-0.2 mm
Chamotte (percentage)
25 %
Firing range (°C)
1000 - 1120
Drying shrinkage (110°C)
8 %
firing shrinkage at 1070°C
5 %
firing shrinkage at 1140°C
7 %
firing shrinkage at 1200°C / 1240°C
/
Appropriate for throwing
yes
Appropriate for pressing / stamping
yes
Appropriate for modelling / stamping
yes
Water absorption at 1070°C
11 %
Water absorption at 1140°C
7 %
Water absorption at 1200 / 1240°C
5 %
Coefficient of thermal expansion WAK x 10 -7 °C -1 (pre-firing at 1000°C) 20 - 500
57 at 1240 °C
Color after firing
gray - black
Chamotte (size)
0.2 - 0.8 mm
Chamotte (addition in %)
30 %
Firing temperature
1000 - 1240
Shrinkage during drying (110°C)
6 %
Shrinkage during firing at 1070°C
5 %
Shrinkage during firing at 1140°C
7 %
Shrinkage during firing at 1200°C / 1240°C
7 %
Suitable for spindle
/
Suitable for pressing / stamping
/
Suitable for modeling / stamping
yes